Image icon  Al-4 wt% Cu, over aged alloy

 
Use this resource: Use this resource icon
Link to this page: http://core.materials.ac.uk/search/detail.php?id=1689
View at:            
Resource type: Image
Description: Prolonged heat treatment above 150°C to 200°C has led to the evolution of the stable CuAl2 phase (θ). The CuAl2 phase is visible at high magnifications. It does not contribute to the strength of the alloy and the over aged aluminium has poor mechanical properties.
Keywords: aged • alloy • aluminium • copper • hardening • heat treatment • metal • quenching • vacancy
Categories: Science approaches > Microstructure
Materials > Metals & alloys > Aluminium & alloys
Materials > Metals & alloys > Copper & alloys
Processes > Thermal treatments > Ageing
Testing, analysis & experimentation > Metallography
Scale > Micro
Created by: Dr J Marrow, Department of Materials Science, University of Manchester and UMIST
DoITPoMS, University of Cambridge
Published by: DoITPoMS, University of Cambridge
License: This resource is released under the Creative Commons Attribution Non-Commercial Share Alike license (2.0 UK: England & Wales).
Creative Commons Attribution Non-Commercial Share Alike logo
You are free:
  • to share – to copy, distribute and transmit the work
  • to remix – to adapt the work
Under the following conditions:
  • attribution – You must attribute the work in the manner specified by the author or licensor (but not in any way that suggests that they endorse you or your use of the work).
  • noncommercial – You may not use this work for commercial purposes.
  • share alike – If you alter, transform, or build upon this work, you may distribute the resulting work only under the same or similar license to this one.
View the full legal code here.
Date created: 07 November 2002
Date added: 21 August 2009
Package:
Resource ID: 1689